Hong Ye Jie Tech Co., LTD
Hong Ye Jie Tech Co., LTD
Molding Silicone Rubber
  • Molding Silicone Rubber
  • Molding Silicone Rubber
  • Molding Silicone Rubber
  • Molding Silicone Rubber
  • Molding Silicone Rubber
Molding Silicone Rubber
Molding Silicone Rubber
Molding Silicone Rubber
Molding Silicone Rubber
Molding Silicone Rubber

Molding Silicone Rubber

Quantity:

Your message must be between 20 to 2000 characters

Contact Now
Basic Info
Basic Info
Product Description
Product Description

Molding Silicone Rubber  Description:
Molding Silicone Rubber HY620 is mainly used for toy gifts and craftwork gifts with the advantages of good tensile strength, high tear strength, high temperature resistance, high duplication times and repeated use, etc. It is suitable for small products or fine and precision products which is difficult to demould. This molding Silicone Rubber is one of the products with the highest use level in the production of craftwork gifts and the shrinkage is up to 2‰.

 

Molding Silicone Rubber  Standard Datasheet:

Model Appearance Viscosity (cps) Hardness (A°) Tensile strength (Mpa) Tear strength (KN/m) Elongation (%) Mixing ratio (%) Operating time(H) Curing time(H)
620 White ≤16000 20±2 ≥2.8 ≥20 ≥400 2~3 0.5~1 2~5

 

Molding silicone rubber Operation Instruction:
Molding silicone rubber  is white or red flowing liquid with general hardness of 18-22A°after curing . If the customer wants to make large products and large size molds, the mold should be made of silica gel with high hardness. On the contrary, if the mold with fine and precision patterns , it should be made of liquid silicone with low hardness. The amount of the curing agent depends on the actual requirements of the customer. If molds requiring fast drying and demould, more curing agent is needed; contrarily, if molds requiring slower drying and demould, less curing agent is needed.
(Note: our company does not recommend you to add silicone oil. If a special soft liquid silicone mold or fine detailed and complex patterns products are required, 5%-10% silica gel oil can be added to soften the mold for easy demould.)

 

Molding Silicone Rubber FAQ:
Why is the appearance of the finished mold striate and unsmooth?
It is because the appearance of the product or the model itself is not perfect, and it has not been polished before the further operation. So when you make silicon molds, firstly you should polish the products, spray the realese agent evenly on the product. In this case, the problem can be avoided.

 

Any further information pls feel free to contact with Ms Nina
TEL: 0086-755-89948019
Fax: 0086-755-89948030
E-mail: hyjr(at)szrl(dot)net
Website: www(dot)szrl(dot)net

Send your message to this supplier

  • Ms. Nina

  • Enter between 20 to 4,000 characters.